I have been making knives for some years and recently heat treated a batch of ATS-34 blades in my furnace. I quenched between aluminum plates in a vise after a soak of 1975-2000 degrees. When I attempted to surface grind, the blades were no longer attracted to a magnet. What did I do wrong? Is my pyrometer miscalibrated?